Add to Cart
gas shielded welding wire
1.fast depositing speed
2.high depositing efficiency
3.stable arc
Chemical composition:
C | Mn | Si | S | P | Cu | Other | |
standard value | 0.06-0.15 | 1.40-71.85 | 0.80-1.15 | ≤0.035 | ≤ 0.025 | ≤ 0.50 | ≤ 0.50 |
sample value | 0.08 | 1.51 | 0.92 | 0.020 | 0.016 | 0.20 | 0.02 |
Typical mechanical properties of deposited metal:
Tenile strength | Yield point δ0.2(MPa) | Elongation | AKV Impact value | Shielding gas |
≥ 500 | ≥ 420 | ≥ 22 | ≥ 27 | 100%CO2 |
560 | 500 | 27 | 102 | 100%CO2 |
Diameter of wire & referance current(DC+)
Diameter of wire (mm) | Ø0.8 | Ø 1.0 | Ø 1.2 | Ø 1.6 |
F current (A) | 40-180 | 50-220 | 80-350 | 170-550 |
V current (A) | 40-140 | 50-160 | 50-180 | |
OH current (A) | 40-120 | 50-160 | 45-180 |